Metal has been mild steel 3/16" square tube, just running beads on one side, sometimes with filler. Filler is er70s2.
I have the tried gas from 5-40cu/ft/hr all with similar results. HF start works good almost always. I'm holding the torch about 3/16" from surface, and at about 15-20deg angle. I hear the purge of gas when I light off. I've put soapy water around line connections that I can see and no bubbling. I clean the tungsten and the metal ground off shiney with acetone.
So for now I'm lost. Mostly I've been trying in the 80-100amp range. I had some thinner plate I tried at 60Amps, all looks the same.
I've also tried some 3/16" aluminum plate on AC and it was pretty much worse then the mild steel. I couldn't even get filler to add to the crappy puddle.
Any thoughts?
My only somewhat decent bead. Still horrible

Most look like this


Heres the tungsten before a spot test

Here it is dirty after a 5sec light up and 10sec post flow.

Heres some spot test, one on the left I had it lit for 10 seconds.